Thermal Analysis Evaluation System
Differential Scanning Calorimeter
DSC-R series
ULVAC EQUIPMENT SALES

Print/Download
For more information on ULVAC products, purchase, and/or consideration, click here.
A high-sensitivity sensor is standard equipment on all models
Achieves a high-stability baseline through its precise thermal design.
Achieves a high-stability baseline through its precise thermal design.
Features
- Capable of easily measuring the specific heat capacity of solids and powders
Applications
- Measures the glass transition point of polymer materials
- Melting point determination of low-melting point metals such as solders
- Measures the transformation point of metallic materials
- Measures the specific heat capacity of solid (powdered) materials
Specifications
Model | DSC-R | DSC-RL | DSC-RS |
---|---|---|---|
Temperature Range | RT ~ 650℃ | -150 ~ 650℃ | -150 ~ 650℃ Cycled heating and cooling |
Sample Vessel Size | Aluminum: Φ5 mm x 5 mm thick, 0.05 cc | ||
Measurement Atmosphere | Air, inert gas |